Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 2.37 J | 1.75 ft-lb | ASTM D5420 |
RheTech Products FRP300-00 20% Talc Reinforced Polypropylene Copolymer, Flame Retardant, Natural Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 2.37 J | 1.75 ft-lb | ASTM D5420 |
RheTech Products FRP300-01 20% Talc Reinforced Polypropylene Copolymer, Flame Retardant, Black Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products. |