Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 15.9 J | 11.7 ft-lb | ASTM D5420 |
RheTech Products FT4802-691UV Thermoplastic Polyolefin, UV Stabilized, RJ3 Dark Grey Green Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 15.9 J | 11.7 ft-lb | ASTM D5420 |
RheTech Products FT4802-692UV Thermoplastic Polyolefin, UV Stabilized, RS8 Grey Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 15.9 J | 11.7 ft-lb | ASTM D5420 |
RheTech Products FT4802-693UV Thermoplastic Polyolefin, UV Stabilized, SPN Dark Teal Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |