Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 21.0 J @Temperature -30.0 °C |
15.5 ft-lb @Temperature -22.0 °F |
ASTM D3029 |
LyondellBasell Hifaxâ„¢ CA199AC Thermoplastic Olefin Resin Key Features: low melt flow, medium low modulus, paintable thermoplastic olefin resin, excellent balance of properties, high toughness, good paintability, flexibleApplications: automotive air bag do.. |
|||
Gardner Impact | 21.0 J | 15.5 ft-lb | ASTM D3029 |
SABIC Innovative Plastics NORYL SPN410 PPE+PS Improved productivity. 210F (99C) DTUL. UL94 HB rated. |
|||
Gardner Impact | 21.0 J | 15.5 ft-lb | ASTM D3029 |
SABIC Innovative Plastics ULTEM 1100F PEI Standard flow Polyetherimide (Tg 217C). ECO Conforming. US FDA and EU Food Contact compliant. UL94 V0, V2 and 5VA listing. Effective June 2007, this grade will no longer be supported with biocompa.. |
|||
Gardner Impact | 21.0 J | 15.5 ft-lb | ASTM D3029 |
SABIC Innovative Plastics ULTEM 1100F PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant. Effective June 2007, this grade will no longer be supported with biocompati.. |
|||
Gardner Impact | 21.0 J @Temperature 23.0 °C |
15.5 ft-lb @Temperature 73.4 °F |
ASTM D 3029 |
SABIC Innovative Plastics Ultem 1100R PEI Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Gardner Impact | 21.0 J @Temperature 23.0 °C |
15.5 ft-lb @Temperature 73.4 °F |
ASTM D 3029 |
SABIC Innovative Plastics Ultem 1100R PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Gardner Impact | 21.0 J @Temperature 23.0 °C |
15.5 ft-lb @Temperature 73.4 °F |
ASTM D 3029 |
SABIC Innovative Plastics Ultem MD130A PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Americas region. |
|||
Gardner Impact | 21.0 J @Thickness 3.17 mm, Temperature -30.0 °C |
15.5 ft-lb @Thickness 0.125 in, Temperature -22.0 °F |
ASTM D5420 |
ExxonMobil PP7035E4 Impact Copolymer Product Description: A medium impact copolymer resin designed for injection molding applications requiring high melt flow rate.Availability: North America Features:Good ColorablityGood Dimensional .. |
|||
Gardner Impact | 21.0 J @Temperature -30.0 °C |
15.5 ft-lb @Temperature -22.0 °F |
ASTM D3029 |
LyondellBasell Astryn 7523C Polypropylene Copolymer Key Features: conventional melt flow, medium modulus polypropylene copolymer, excellent impact and stiffness balance, excellent chemical resistance, versatile, good processabilityApplications: autom.. |