Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 11.3 J | 8.33 ft-lb | ASTM D5420-93 |
Multibase Multi-Pro® 3216 CUW BLK Polypropylene Multi-Pro 3216 CUW BLK is well suited for resin furniture requiring high impact strength and stiffness at moderate cost.Data provided by Multibase. |
|||
Gardner Impact | 11.3 J | 8.33 ft-lb | ASTM D5420-93 |
Multibase Multi-Pro® 4013 CU Yellow 40% Filler Content Polypropylene Data provided by Multibase. |
|||
Gardner Impact | 11.3 J | 8.33 ft-lb | ASTM D5420 |
PolyOne OnForce™ LFT AM-40LGF/001 Natural Polyphthalamide (PPA) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Gardner Impact | 11.3 J | 8.30 ft-lb | ASTM D5420 |
RheTech Products T20P200-01BG 20% Talc Reinforced Polypropylene Copolymer, General Purpose Black, Blow Molding Grade Applications: HVAC ductsSeat backsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 11.3 J | 8.33 ft-lb | ASTM D3029 |
Polymer Resources PC-HH Polycarbonate, High Heat Polycarbonate, High HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resource.. |
|||
Gardner Impact | 11.3 J | 8.33 ft-lb | ASTM D3029 |
Polymer Resources PC-HH-UV Polycarbonate, High Heat, UV-stabilized Polycarbonate, High Heat, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P.. |
|||
Gardner Impact | >= 11.3 J | >= 8.33 ft-lb | |
Buckeye Polymers BP PPC 0212 R Reprocessed Polypropylene, Unfilled Blk/WhiteThis reprocessed product is successful in applications where cost is a major specification, yet physical characteristics require product performance. Industrial recycled resin compounds ar.. |
|||
Gardner Impact | 11.3 J | 8.33 ft-lb | ASTM D3029 |
Adell RZ-16 Copolymer Polypropylene, 30% Calcium Carbonate Filled Data provided by Adell Plastics, Inc. |
|||
Gardner Impact | 11.3 J | 8.33 ft-lb | ASTM D3029 |
Buckeye Polymers BP RPP 4012 C Polypropylene, 40% Mineral Filled Calcium carbonate-filled PP grades have a high impact toughness, moderate increased stiffness, and excel in high gloss applications. This material can be customized through the addition of UV packag.. |