Mechanical Properties Metric English Comments
Gardner Impact 0.904 J
0.667 ft-lb
ASTM D5420
RheTech Products F43-01A 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: Electrical component supportsFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 0.904 J
0.667 ft-lb
ASTM D5420
RheTech Products F52-01 20% Mica Reinforced Polypropylene Copolymer, Black
Applications: Functional support ductsHousingsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 0.904 J
0.667 ft-lb
ASTM D5420
RheTech Products FRP102-00 Polypropylene, Flame Retardant, Natural
Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 0.904 J
0.667 ft-lb
ASTM D5420
RheTech Products FRP102-01 Polypropylene, Flame Retardant, Black
Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 0.904 J
0.667 ft-lb
ASTM D5420
RheTech Products GC45P200-01UV 45% Glass Fiber Reinforced Polypropylene Copolymer, UV Stabilized, Black
Applications: BracketsUnderhood componentsLarge structural supportsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 0.904 J
0.667 ft-lb
ASTM D5420
RheTech Products T10P100-00 10% Talc Reinforced Polypropylene, Natural
Applications: Consumer goodsIP structural componentsInterior trimInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 0.904 J
0.667 ft-lb
ASTM D5420
RheTech Products T10P100-01 10% Talc Reinforced Polypropylene, Black
Applications: Consumer goodsAir ductsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 0.904 J
0.667 ft-lb
ASTM D5420
RheTech Products T10UP100-01 10% Talc Reinforced Polypropylene Copolymer, General Purpose Black, UL94 HB Rated
Applications: Wire troughElectrical componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 0.904 J
0.667 ft-lb
ASTM D5420
RheTech Products T40P100-00A 40% Talc Reinforced Polypropylene, Natural
Applications: Durable goodsHVAC componentsFunctional supportsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 0.904 J
0.667 ft-lb
ASTM D5420
RheTech Products T40P100-01 40% Talc Reinforced Polypropylene, Black
Applications: Wire troughBracketsConsolesFan shroudsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 0.904 J
0.667 ft-lb
ASTM D5420
RheTech Products T40P100-01A 40% Talc Reinforced Polypropylene, Black
Applications: Wire troughBracketsConsolesFan shroudsFuse panel boxInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 0.904 J
0.667 ft-lb
ASTM D5420
RheTech Products T40P100-774UVA 40% Talc Reinforced Polypropylene, UV Stabilized, JA6A Black
Applications: Wire troughBracketsConsolesFan shroudsFuse panel boxDoor cup pullsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 0.904 J
0.667 ft-lb
ASTM D5420
RheTech Products T40P105-01 40% Talc Reinforced Polypropylene, Black
Applications: Underhood componentsHVAC ductworkInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 0.904 J
0.667 ft-lb
ASTM D5420
RheTech Products T40P106-01 40% Talc Reinforced Polypropylene, Black
Applications: Underhood componentsHVAC ductworkFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 0.904 J
0.667 ft-lb
ASTM D5420
RheTech Products T40P108-01 40% Talc Reinforced Polypropylene, Black
Applications: Wire troughBracketsConsolesFan shroudsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 0.904 J
0.667 ft-lb
ASTM D5420
RheTech Products T40P108-01A 40% Talc Reinforced Polypropylene, Black
Applications: Underhood componentsHVAC ductworkFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 0.904 J
0.667 ft-lb
ASTM D5420
RheTech Products T40P109-01 40% Talc Reinforced Polypropylene, Black
Applications: Underhood componentsHVAC ductworkBrackets/SupportsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 0.904 - 40.7 J
0.667 - 30.0 ft-lb
Average value: 11.5 J Grade Count:48
Overview of materials for Polypropylene, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri..
Gardner Impact <= 0.904 J

@Temperature 23.0 °C
<= 0.667 ft-lb

@Temperature 73.4 °F
ASTM D5420
Flint Hills P4C5B-181B Polypropylene Homopolymer
Features: Nucleated and Antistat. Product does not contain animal derived components. Phthalate-free.Applications: Injection Molding: Closures and cutleryInformation Provided by Flint Hills Resour..
Gardner Impact 0.904 J
0.667 ft-lb
ASTM D3029
Plastics Group Polifil® GFRMPPCC-30 30% Glass Reinforced Polypropylene, High Impact
Polifil® GFRMPPCC series compounds are high impact polypropylenes reinforced with chemically coupled glass fibers. This combination provides higher impact strength while retaining high stiffness.Ap..
Gardner Impact 0.904 J

@Temperature 23.0 °C
0.667 ft-lb

@Temperature 73.4 °F
ASTM D5420
Washington Penn High Modulus Polypropylene Homopolymer 40% Glass Filled
Mica-filled polypropylene compounds provide the best strength and modulus of any of the particulate fillers which results in an outstanding balance of properties. Mold shrinkage is similar to ABS a..
Gardner Impact 0.904 J

@Temperature 23.0 °C
0.667 ft-lb

@Temperature 73.4 °F
ASTM D5420
Washington Penn High Modulus Polypropylene Homopolymer 40% Glass/Mica Filled
Mica-filled polypropylene compounds provide the best strength and modulus of any of the particulate fillers which results in an outstanding balance of properties. Mold shrinkage is similar to ABS a..
Gardner Impact 0.904 J

@Temperature 23.0 °C
0.667 ft-lb

@Temperature 73.4 °F
ASTM D5420
Washington Penn Homopolymer Polypropylene 10% Talc Filled
Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requi..
Gardner Impact 0.904 J

@Temperature 23.0 °C
0.667 ft-lb

@Temperature 73.4 °F
ASTM D5420
Washington Penn Homopolymer Polypropylene 20% Glass Reinforced
Fiberglass & mineral-reinforced polypropylene compounds provide excellent tensile and impact properties. Mold shrinkage is similar to ABS and polystyrene. Compounds also have dimensional stability. ..
Gardner Impact 0.904 J

@Temperature 23.0 °C
0.667 ft-lb

@Temperature 73.4 °F
ASTM D5420
Washington Penn Homopolymer Polypropylene 20% Talc Filled
Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requi..
Gardner Impact 0.904 J

@Temperature 23.0 °C
0.667 ft-lb

@Temperature 73.4 °F
ASTM D5420
Washington Penn Homopolymer Polypropylene 27% Glass Reinforced
Fiberglass & mineral-reinforced polypropylene compounds provide excellent tensile and impact properties. Mold shrinkage is similar to ABS and polystyrene. Compounds also have dimensional stability. ..
Gardner Impact 0.904 J
0.667 ft-lb
ASTM D3029
Plastics Group Polifil® GFPP-10 10% Glass-Reinforced Polypropylene
Polifil® GFPP series compounds are homopolymer polypropylene resins reinforced with glass fibers. They provide high impact with increased strength, stiffness, surface hardness, and higher continuou..
Gardner Impact 0.904 J
0.667 ft-lb
ASTM D3029
Plastics Group Polifil® GFPPCC-10 10% Glass Reinforced Polypropylene
Polifil® GFPPCC series compounds are homopolymer polypropylenes reinforced with chemically coupled glass fibers. These compounds offer superior strength and stiffness, improved elevated temperature..
Gardner Impact 0.904 - 260 J
0.667 - 192 ft-lb
Average value: 26.8 J Grade Count:24
Overview of materials for Polypropylene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of..
Gardner Impact 0.904 J
0.667 ft-lb
ASTM D5420
RheTech Products G20P252-00 20% Glass Fiber Reinforced Polypropylene Copolymer, Natural
Applications: Interior trimArm rest insertConsolesDome light housingInjection molding conditions reported in table.Information provided by RheTech Products.