Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Total Energy | 55.0 J/cm @Temperature 23.0 °C |
0.103 ft-lb/mil @Temperature 73.4 °F |
|
Mapal Plastics Maplon Type O Polypropylene Sheet Properties: Corona treated on both sides for offset and screen printing, Extended shelf life, Low stress whitening, Suitable for die cuttingApplications: Stationery products, Offset printed item |
|||
Dart Drop Total Energy | 55.0 J/cm @Temperature 23.0 °C |
0.103 ft-lb/mil @Temperature 73.4 °F |
|
Mapal Plastics Maplon Type S Polypropylene Sheet Properties: Low stress whitening, Suitable for die cutting, Corona treated on both sides for offset and screen printingApplications: Stationery, Packaging, House-hold productsand printed items |
|||
Dart Drop Total Energy | 55.0 - 60.0 J/cm | 0.103 - 0.112 ft-lb/mil | Average value: 56.7 J/cm Grade Count:3 |
Overview of materials for Polypropylene, Sheet/Thermoforming Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Sheet/Thermoforming Grade". Each property range of values reported is minimum and maximum.. |