Mechanical Properties Metric English Comments
Dart Drop Total Energy 890 J/cm
1.67 ft-lb/mil
Puncture Resistance; SABIC Method
SABIC 518N Linear Low Density Polyethylene for Blown Film
Product Description: 548N is a fractional melt index Linear Low Density Polyethylene grade suitable for high strength packaging applications. Films produced using this resin yield outstanding toug..
Dart Drop Total Energy 890 J/cm
1.67 ft-lb/mil
Puncture Resistance; SABIC Method
SABIC 6821N Linear Low Density Polyethylene for Blown Film
Product Description: 6821N is a fractional melt index hexene copolymer based Linear Low Density Polyethylene grade suitable for high strength packaging applications. Films produced using this resi..