Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Total Energy | 620 J/cm | 1.16 ft-lb/mil | Puncture Resistance; SABIC Method |
SABIC 726 Series Linear Low Density Polyethylene for Blown Film Product Description: 726 series resins are fractional index Linear Low Density Polyethylene grades suitable for blown film applications. Films produced using these resins give a relatively higher .. |