Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Total Energy | 380 J/cm | 0.712 ft-lb/mil | DIN 53373 |
BASF Ecovio® C2224 F Blend Biodegradable Polyester Description: Ecovio® F Blend C2224 is our biodegradable film product containing renewable resources. It is basically a compound of our biodegradable copolyester Ecoflex® F Blend and polylactic aci.. |