Mechanical Properties | Metric | English | Comments |
---|---|---|---|
200% Modulus | 0.00758 GPa | 1.10 ksi | ASTM D412 |
Techmer ES HiFill® TPU 85A 0152 S1 Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalInformation provided by TP Composites, Inc. |
|||
200% Modulus | 0.00760 GPa | 1.10 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 5565 Dense Extruded Profile FormulationNordel® IP 5565 |