Mechanical Properties Metric English Comments
200% Modulus 0.00498 GPa
0.723 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Carbon Black, N-550 (FEF)
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
200% Modulus 0.00498 GPa
0.723 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 40 PHR Carbon Black, N-774 (SRF)
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
200% Modulus 0.00498 GPa
0.723 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 60A, Black Sulfur Cure
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
200% Modulus 0.00498 GPa
0.723 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Carbon Black, N-550 (FEF)
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
200% Modulus 0.00498 GPa
0.723 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 40 PHR Carbon Black, N-774 (SRF)
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
200% Modulus 0.00498 GPa
0.723 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 60A, Black Sulfur Cure
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..