Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact Resistance | 2.70 J/cm² | 12.8 ft-lb/in² | |
Dow DOWLEX™ IP-40 High Density Polyethylene DOWLEX® IP-40 resin is an improved processing high density resin designed to offer excellent processability and impact resistance required for food container applications. This resin is designed by.. |
|||
Izod Impact Resistance | 2.70 J/cm² | 12.8 ft-lb/in² | |
Dow DOWLEX™ IP-50 High Density Polyethylene DOWLEX® IP-50 resin is an improved processing high density polyethylene resin with controlled molecular weight distribution designed for thin wall food containers. This resin is recommended for flo.. |