Polymer Property : Puncture Energy = 47.9 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 65.0 J

@Load <=510 kg,
Temperature 23.0 °C
47.9 ft-lb

@Load <=1120 lb,
Temperature 73.4 °F
ISO 6603-2
Lanxess Durethan® BC 550 Z DUSXBL 900116 Nylon 6, Impact Modified
PA 6, non-reinforced, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS.
Puncture Energy 65.0 J

@Temperature 0.000 °C
47.9 ft-lb

@Temperature 32.0 °F
at Max load; ASTM D3763
Eastman Tritan TX1800 Copolyester
Applications:Consumer and durable goodsExtrusion blow moldingInjection stretch blow moldingKey Attributes:Ease of processingExcellent clarityExcellent Hydrolytic stabilityGood chemical resistanceGoo..
Puncture Energy 65.0 J

@Temperature 0.000 °C
47.9 ft-lb

@Temperature 32.0 °F
at Max load; ASTM D3763
Eastman Tritan TX1801 Copolyester, Natural
Applications:Consumer and durable goodsExtrusion blow moldingInjection stretch blow moldingKey Attributes:Ease of processingExcellent clarityExcellent Hydrolytic stabilityGood chemical resistanceGoo..
Puncture Energy 65.0 J

@Temperature 0.000 °C
47.9 ft-lb

@Temperature 32.0 °F
Energy @ Max. Load; ASTM D3763
Eastman Tritan WX500 Copolyester
Eastman Tritan WX500 is a resin specifically developed for blow molded bottles. Extremely high melt strength makes the resin an excellent choice when manufacturing large bottles. This new-generati..
Puncture Energy 65.0 J

@Temperature 0.000 °C
47.9 ft-lb

@Temperature 32.0 °F
Energy @ Max. Load; ASTM D3763
Eastman Tritan WX510 Copolyester
Eastman Tritan WX510 is a transparent blue resin specifically developed for blow molded bottles. Extremely high melt strength makes the resin an excellent choice when manufacturing large bottles. ..
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 1952 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardancy• Me..
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 2400 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low..
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 2405 MAS048 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low..
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 2407 MAS070 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low..
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 2407 MAS145 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low..
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 2408 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc..
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 2600 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 2607 MAS167 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 2652 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•..
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 2665 MAS071 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med..
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 2665 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medium viscosity, easy..
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 2667 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med..
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 2800 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 2805 MAS145 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 2805 MAS152 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
Puncture Energy 65.0 J

@Temperature 23.0 °C
47.9 ft-lb

@Temperature 73.4 °F
ISO 6603-2
Covestro Makrolon® 3258 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc..
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® FU1007 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Furniture applications..
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® Rx2435 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices• Low..
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® ET2613 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• Medium vi..
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® ET3127 Polycarbonate
Makrolon® polycarbonate resinMain characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characterist..
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® ET3227 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• High visc..
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® LED2643 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• LED lighting, optics, ..
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® LQ2647 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Optical lens, safety g..
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® Rx1851 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices• Low..