Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 30.0 J @Temperature 0.000 °C |
22.1 ft-lb @Temperature 32.0 °F |
ISO 6603-2 |
Borealis BC142MO Polypropylene Copolymer BC142MO is a controlled rheology polypropylene heterophasic copolymer. It is characterized by high impact strength, good stiffness, excellent process ability, good flow properties and low warpage. .. |
|||
Puncture Energy | 30.0 J @Temperature 0.000 °C |
22.1 ft-lb @Temperature 32.0 °F |
ISO 6603-2 |
Borealis BH345MO Polypropylene Copolymer BH345MO is a heterophasic copolymer. This grade is characterized by optimum combination of very high stiffness, good flow properties and good impact strength. and is designed for high speed injectio.. |
|||
Puncture Energy | 30.0 J @Temperature 0.000 °C |
22.1 ft-lb @Temperature 32.0 °F |
ISO 6603-2 |
Borealis BJ360MO Polypropylene Copolymer BJ360MO is a heterophasic copolymer. This grade provides unique combination of very high melt flow rate, high impact strength and stiffness. and is designed for high-speed injection molding and cont.. |