Polymer Property : Puncture Energy = 22.1 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 30.0 J

@Temperature 0.000 °C
22.1 ft-lb

@Temperature 32.0 °F
ISO 6603-2
Borealis BC142MO Polypropylene Copolymer
BC142MO is a controlled rheology polypropylene heterophasic copolymer. It is characterized by high impact strength, good stiffness, excellent process ability, good flow properties and low warpage. ..
Puncture Energy 30.0 J

@Temperature 0.000 °C
22.1 ft-lb

@Temperature 32.0 °F
ISO 6603-2
Borealis BH345MO Polypropylene Copolymer
BH345MO is a heterophasic copolymer. This grade is characterized by optimum combination of very high stiffness, good flow properties and good impact strength. and is designed for high speed injectio..
Puncture Energy 30.0 J

@Temperature 0.000 °C
22.1 ft-lb

@Temperature 32.0 °F
ISO 6603-2
Borealis BJ360MO Polypropylene Copolymer
BJ360MO is a heterophasic copolymer. This grade provides unique combination of very high melt flow rate, high impact strength and stiffness. and is designed for high-speed injection molding and cont..