Polymer Property : Secant Modulus = 958 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 6.61 GPa

@Strain 1.68 %,
Temperature 40.0 °C
958 ksi

@Strain 1.68 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® FR530 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
30% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR530 NC010 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont ..
Secant Modulus 6.60 GPa

@Strain 0.900 %,
Temperature 100 °C
958 ksi

@Strain 0.900 %,
Temperature 212 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 51G45HSL NC010 Polyphthalamide (PPA)  (Unverified Data**)
45% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G45HSL NC010 is a 45% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information ..