Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 6.60 GPa @Strain 1.84 %, Temperature 23.0 °C |
957 ksi @Strain 1.84 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9330 NC010 PBT+SAN
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9330 NC010 is a 30% glass fiber reinforced polybutylene terephthalate blend for injection molding. I.. |
|||
Secant Modulus | 6.60 GPa @Strain 0.100 %, Temperature 100 °C |
957 ksi @Strain 0.100 %, Temperature 212 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® FR50 NC010A Nylon 66
(Unverified Data**) 25% Glass Reinforced Flame Retardant Polyamide 66 Zytel FR50 NC010A is a 25% glass fiber reinforced flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performanc.. |
|||
Secant Modulus | 6.60 GPa @Strain 0.600 %, Temperature 23.0 °C |
957 ksi @Strain 0.600 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 51G15HSL NC010 Polyphthalamide (PPA)
(Unverified Data**) 15% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G15HSL NC010 is a 15% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information .. |