Polymer Property : Secant Modulus = 923 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 6.36 GPa

@Strain 2.30 %,
Temperature 100 °C
923 ksi

@Strain 2.30 %,
Temperature 212 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 51G35HSLR BK420 Polyphthalamide (PPA)  (Unverified Data**)
35% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G35HSLR BK420 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin with improved hydrolysis resistance..
Secant Modulus 6.36 GPa

@Strain 2.70 %,
Temperature 23.0 °C
923 ksi

@Strain 2.70 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® PLS 95G40DH1T BK261 Nylon 6  (Unverified Data**)
40% Glass Reinforced Heat Stabilized Polyamide Zytel PLS95G40DH1T is a 40% GR impact modified PA made with SHIELD technology its superior heatInformation provided by DuPont Performance Polymers