Polymer Property : Secant Modulus = 9.19 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 9.19 GPa

@Strain 1.48 %,
Temperature 0.000 °C
1330 ksi

@Strain 1.48 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® FR530 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
30% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR530 NC010 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont ..
Secant Modulus 9.19 GPa

@Strain 1.30 %,
Temperature 23.0 °C
1330 ksi

@Strain 1.30 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 73G35HSL BK262 Nylon 6  (Unverified Data**)
35% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G35HSL BK262 is a 35% glass fiber reinforced heat stabilized black polyamide 6 resin for injection molding.Information provided by DuPont Per..