Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 5.79 GPa @Strain 1.50 %, Temperature 23.0 °C |
839 ksi @Strain 1.50 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK643FR NC010 Polybutylene Terephthalate (PBT) 20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK643FR is a flame retardant 20% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.8.. |
|||
Secant Modulus | 5.78 GPa @Strain 0.900 %, Temperature 40.0 °C |
839 ksi @Strain 0.900 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Sorona® 3015G NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& 15% Glass Reinforced Polytrimethylene Terephthalate with Resin Made from Bio-PDO Sorona 3015G NC010 is a 15% glass reinforced PTT resin containing 31% renewably sourced ingredients by weight (37% ba.. |