Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 4.83 GPa @Strain 1.71 %, Temperature 40.0 °C |
701 ksi @Strain 1.71 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® HR5330HFS BK591 Polybutylene Terephthalate (PBT)
(Unverified Data**) 30% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5330HFS is a 30% glass fiber reinforced moderately toughened hydrolysis resistant polybutylene terephthalate for inject.. |
|||
Secant Modulus | 4.83 GPa @Strain 1.71 %, Temperature 40.0 °C |
701 ksi @Strain 1.71 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® HR5330HFS NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate with Improved Processing Crastin HR5330HFS is a 30% glass fiber reinforced moderately toughened hydrolysis resistant polybutylene terephthalate for in.. |
|||
Secant Modulus | 4.84 GPa @Strain 0.700 %, Temperature 100 °C |
701 ksi @Strain 0.700 %, Temperature 212 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN FR52G30NH NC010 Polyphthalamide (PPA)
(Unverified Data**) 30% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide Zytel HTNFR52G30NH NC010 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin. It.. |