Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 5.95 GPa @Strain 1.80 %, Temperature 23.0 °C |
863 ksi @Strain 1.80 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 51G15HSL NC010 Polyphthalamide (PPA)
(Unverified Data**) 15% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G15HSL NC010 is a 15% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information .. |