Mechanical Properties Metric English Comments
Secant Modulus 5.48 GPa

@Strain 0.250 %,
Temperature -40.0 °C
795 ksi

@Strain 0.250 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK601 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
10% Glass Reinforced Polybutylene Terephthalate Crastin SK601 NC010 is a 10% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P..
Secant Modulus 5.48 GPa

@Strain 1.30 %,
Temperature 23.0 °C
795 ksi

@Strain 1.30 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Sorona® 3015G NC010 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)&
15% Glass Reinforced Polytrimethylene Terephthalate with Resin Made from Bio-PDO Sorona 3015G NC010 is a 15% glass reinforced PTT resin containing 31% renewably sourced ingredients by weight (37% ba..
Copyright © lookpolymers.com All Rights Reserved