Polymer Property : Secant Modulus = 5.46 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 5.46 GPa

@Strain 1.80 %,
Temperature 0.000 °C
792 ksi

@Strain 1.80 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Sorona® 3015G NC010 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)&
15% Glass Reinforced Polytrimethylene Terephthalate with Resin Made from Bio-PDO Sorona 3015G NC010 is a 15% glass reinforced PTT resin containing 31% renewably sourced ingredients by weight (37% ba..
Secant Modulus 5.46 GPa

@Strain 0.294996 %,
Temperature 80.0 °C
793 ksi

@Strain 0.294996 %,
Temperature 176 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK615SF NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
30% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK615SF is a 30% glass fiber reinforced low viscosity polybutylene terephthalate for injecti..