Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 5.23 GPa @Strain 1.70 %, Temperature 23.0 °C |
758 ksi @Strain 1.70 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Sorona® 3015G NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& 15% Glass Reinforced Polytrimethylene Terephthalate with Resin Made from Bio-PDO Sorona 3015G NC010 is a 15% glass reinforced PTT resin containing 31% renewably sourced ingredients by weight (37% ba.. |