Mechanical Properties Metric English Comments
Secant Modulus 3.56 GPa

@Strain 0.900 %,
Temperature -20.0 °C
516 ksi

@Strain 0.900 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500AF Acetal (POM)  (Unverified Data**)
20% Teflon® Fiber Filled Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500AF is a medium viscosity acetal homopolymer resin containing 20% Teflon PTFE fibers. It is desi..
Secant Modulus 3.56 GPa

@Strain 2.80 %,
Temperature 23.0 °C
516 ksi

@Strain 2.80 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 510GR NC000 Acetal (POM)  (Unverified Data**)
10% Glass Reinforced Medium Viscosity Acetal Homopolymer Delrin 510GR is a 10% glass reinforced acetal homopolymer for injection molding. It has high strength stiffness and high deflection temperatu..
Secant Modulus 3.56 GPa

@Strain 0.500 %,
Temperature 0.000 °C
516 ksi

@Strain 0.500 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 511DP NC010 Acetal (POM)  (Unverified Data**)
Nucleated Medium Viscosity Acetal Homopolymer Delrin 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less s..
Secant Modulus 3.56 GPa

@Strain 0.500 %,
Temperature 0.000 °C
516 ksi

@Strain 0.500 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG511DP NC010 Acetal (POM)  (Unverified Data**)
Nucleated Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for mo..
Copyright © lookpolymers.com All Rights Reserved