Polymer Property : Secant Modulus = 282 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 1.95 GPa

@Strain 3.80 %,
Temperature -20.0 °C
282 ksi

@Strain 3.80 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® 6129 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection MoldingInformation provided by DuPont Performance Polymers
Secant Modulus 1.95 GPa

@Strain 3.80 %,
Temperature -20.0 °C
282 ksi

@Strain 3.80 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® 6130 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin 6130 NC010 is an unreinforced medium high viscosity polybutylene terephthalate resin for ..
Secant Modulus 1.94 GPa

@Strain 1.40 %,
Temperature 40.0 °C
282 ksi

@Strain 1.40 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500AF Acetal (POM)  (Unverified Data**)
20% Teflon® Fiber Filled Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500AF is a medium viscosity acetal homopolymer resin containing 20% Teflon PTFE fibers. It is desi..
Secant Modulus 1.94 GPa

@Strain 3.60 %,
Temperature 40.0 °C
282 ksi

@Strain 3.60 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® 415HP NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
15% Glass Reinforced Polyethylene Terephthalate with Excellent Impact Resistance Rynite 415HP NC010 is a 15% glass reinforced modified polyethylene terephthalate improved for easy fast processing ov..