Polymer Property : Secant Modulus = 225 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 1.55 GPa

@Strain 6.14547 %,
Temperature -40.0 °C
225 ksi

@Strain 6.14547 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® S600F10 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin S600F10 NC010 is an unreinforced lubricated medium high viscosity polybutylene terephthal..
Secant Modulus 1.55 GPa

@Strain 1.40 %,
Temperature 40.0 °C
225 ksi

@Strain 1.40 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500T NC010 Acetal (POM)  (Unverified Data**)
Toughened Medium Viscosity Acetal Homopolymer Delrin 500T NC010 is a toughened medium viscosity acetal homopolymer resin with impact resistance similar to Delrin 100. It can be used in parts requiri..
Secant Modulus 1.55 GPa

@Strain 3.87 %,
Temperature 100 °C
225 ksi

@Strain 3.87 %,
Temperature 212 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS 32CG20HSL BK409 Nylon 610  (Unverified Data**)
20% Carbon/Glass Reinforced Renewably Sourced Polyamide 610 Information provided by DuPont Performance Polymers
Secant Modulus 1.55 GPa

@Strain 6.00 %,
Temperature -40.0 °C
225 ksi

@Strain 6.00 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 100 BK602 Acetal (POM)  (Unverified Data**)
High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and ..