Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 1.42 GPa @Strain 5.50 %, Temperature -20.0 °C |
206 ksi @Strain 5.50 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500CL NC010 Acetal (POM)
(Unverified Data**) Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500CL is a medium viscosity acetal homopolymer resin containing a chemical lubricant designed for low wear and fr.. |
|||
Secant Modulus | 1.42 GPa @Strain 0.500 %, Temperature 80.0 °C |
206 ksi @Strain 0.500 %, Temperature 176 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500P BK602 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Improved ProcessingDelrin 500P BK602 is a general purpose medium viscosity black acetal homopolymer resin for injection molding. Delrin 500P has improved pro.. |
|||
Secant Modulus | 1.42 GPa @Strain 4.40 %, Temperature 23.0 °C |
206 ksi @Strain 4.40 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500TL NC010 Acetal (POM)
(Unverified Data**) Teflon® Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500TL is a medium viscosity acetal homopolymer resin containing 1.5% Teflon PTFE Micropowder. It is desi.. |
|||
Secant Modulus | 1.42 GPa @Strain 4.40 %, Temperature 23.0 °C |
206 ksi @Strain 4.40 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG500TL NC010 Acetal (POM)
(Unverified Data**) Teflon® Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact ApplicationsDelrin FG500TL medium viscosity acetal homopolymer resin containing 1.5%.. |
|||
Secant Modulus | 1.42 GPa @Strain 0.230 %, Temperature 23.0 °C |
206 ksi @Strain 0.230 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC3060 NC010 Nylon 610
(Unverified Data**) Unreinforced Renewably Sourced Medium Viscosity Polyamide 610 Developed for Extrusion Zytel RS LC3060 NC010 is a renewable sourced polyamide 610 containing a minimum of 60% renewable sourced ingredi.. |