Mechanical Properties Metric English Comments
Secant Modulus 1.38 GPa

@Temperature 200 °C
200 ksi

@Temperature 392 °F
ASTM D882
DuPont™ Kapton® 250FN029 Polyimide/FEP Composite Film
250 Gauge film structure consisting of a 50 µm (2 mil) base polyimide film with a 13 µm (0.5 mil) coating of Teflon® FEP on one side.Kapton® Type HN film coated with Teflon® FEP fluoropolymer r..
Secant Modulus 1.38 GPa

@Strain 3.23 %,
Temperature -20.0 °C
200 ksi

@Strain 3.23 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® BM6450XD BK560 Polybutylene Terephthalate (PBT)  (Unverified Data**)&
Unreinforced Polybutylene Terephthalate Developed for Blow MoldingCrastin BM6450XD BK560 is an unreinforced supertough polybutylene terephthalate resin with very high viscosity for extrusion and blo..
Secant Modulus 1.38 GPa

@Strain 0.900 %,
Temperature 80.0 °C
200 ksi

@Strain 0.900 %,
Temperature 176 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500TL NC010 Acetal (POM)  (Unverified Data**)
Teflon® Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500TL is a medium viscosity acetal homopolymer resin containing 1.5% Teflon PTFE Micropowder. It is desi..
Secant Modulus 1.38 GPa

@Strain 0.900 %,
Temperature 80.0 °C
200 ksi

@Strain 0.900 %,
Temperature 176 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG500TL NC010 Acetal (POM)  (Unverified Data**)
Teflon® Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact ApplicationsDelrin FG500TL medium viscosity acetal homopolymer resin containing 1.5%..
Secant Modulus 1.38 GPa

@Strain 4.50 %,
Temperature 23.0 °C
200 ksi

@Strain 4.50 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 100 BK602 Acetal (POM)  (Unverified Data**)
High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and ..