Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Secant Modulus = 1460 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 10.1 GPa

@Strain 0.960 %,
Temperature -20.0 °C
1460 ksi

@Strain 0.960 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® LW9030FR NC010 PBT+ASA  (Unverified Data**)
30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030FR NC010 is a 30% glass fiber reinforced flame retardant polybutylene terephthal..
Secant Modulus 10.1 GPa

@Strain 0.110 %,
Temperature -40.0 °C
1460 ksi

@Strain 0.110 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® 935SUV BK593 Polyethylene Terephthalate (PET)  (Unverified Data**)
35% Glass Reinforced UV Stabilized Polyethylene Terephthalate Rynite 935SUV BK593 is a 35% glass fiber /mineral reinforced UV stabilized modified polyethylene terephthalate resin with low warpage de..
Secant Modulus 10.0 GPa

@Strain 0.210 %,
Temperature 40.0 °C
1460 ksi

@Strain 0.210 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® FR530 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
30% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR530 NC010 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont ..
Secant Modulus 10.1 GPa

@Strain 1.86 %,
Temperature 23.0 °C
1460 ksi

@Strain 1.86 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® RE5264 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
36% Glass Reinforced Polyethylene Terephthalate Rynite RE5264 NC010 is a 36% glass fiber reinforced color stabilized modified polyethylene terephthalate.Information provided by DuPont Performance Po..
Secant Modulus 10.1 GPa

@Strain 0.231655 %,
Temperature 0.000 °C
1460 ksi

@Strain 0.231655 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK615SF NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
30% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK615SF is a 30% glass fiber reinforced low viscosity polybutylene terephthalate for injecti..
Secant Modulus 10.1 GPa

@Strain 0.412778 %,
Temperature 23.0 °C
1460 ksi

@Strain 0.412778 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK615SF NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
30% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK615SF is a 30% glass fiber reinforced low viscosity polybutylene terephthalate for injecti..
Secant Modulus 10.0 GPa

@Strain 1.30 %,
Temperature 100 °C
1460 ksi

@Strain 1.30 %,
Temperature 212 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 51G45HSL NC010 Polyphthalamide (PPA)  (Unverified Data**)
45% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G45HSL NC010 is a 45% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information ..
Copyright © lookpolymers.com All Rights Reserved