Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Secant Modulus = 1440 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 9.92 GPa

@Strain 0.660 %,
Temperature -20.0 °C
1440 ksi

@Strain 0.660 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® HR5330HFS BK591 Polybutylene Terephthalate (PBT)  (Unverified Data**)
30% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5330HFS is a 30% glass fiber reinforced moderately toughened hydrolysis resistant polybutylene terephthalate for inject..
Secant Modulus 9.96 GPa

@Strain 0.440 %,
Temperature 0.000 °C
1440 ksi

@Strain 0.440 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® HR5330HFS BK591 Polybutylene Terephthalate (PBT)  (Unverified Data**)
30% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5330HFS is a 30% glass fiber reinforced moderately toughened hydrolysis resistant polybutylene terephthalate for inject..
Secant Modulus 9.92 GPa

@Strain 0.660 %,
Temperature -20.0 °C
1440 ksi

@Strain 0.660 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® HR5330HFS NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
30% Glass Reinforced Polybutylene Terephthalate with Improved Processing Crastin HR5330HFS is a 30% glass fiber reinforced moderately toughened hydrolysis resistant polybutylene terephthalate for in..
Secant Modulus 9.96 GPa

@Strain 0.440 %,
Temperature 0.000 °C
1440 ksi

@Strain 0.440 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® HR5330HFS NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
30% Glass Reinforced Polybutylene Terephthalate with Improved Processing Crastin HR5330HFS is a 30% glass fiber reinforced moderately toughened hydrolysis resistant polybutylene terephthalate for in..
Secant Modulus 9.92 GPa

@Strain 0.250 %,
Temperature -20.0 °C
1440 ksi

@Strain 0.250 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK643FR NC010 Polybutylene Terephthalate (PBT)
20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK643FR is a flame retardant 20% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.8..
Secant Modulus 9.91 GPa

@Strain 0.770 %,
Temperature 23.0 °C
1440 ksi

@Strain 0.770 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® FR530 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
30% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR530 NC010 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont ..
Secant Modulus 9.91 GPa

@Strain 0.340 %,
Temperature -20.0 °C
1440 ksi

@Strain 0.340 %,
Temperature -4.00 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 73G30T NC010 Nylon 6  (Unverified Data**)
30% Glass Reinforced Toughened Polyamide 6 Zytel 73G30T NC010 is a 30% glass fiber reinforced toughened polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Copyright © lookpolymers.com All Rights Reserved