Mechanical Properties Metric English Comments
Secant Modulus 9.16 GPa

@Strain 0.360 %,
Temperature 23.0 °C
1330 ksi

@Strain 0.360 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® HR5330HFS BK591 Polybutylene Terephthalate (PBT)  (Unverified Data**)
30% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5330HFS is a 30% glass fiber reinforced moderately toughened hydrolysis resistant polybutylene terephthalate for inject..
Secant Modulus 9.16 GPa

@Strain 0.360 %,
Temperature 23.0 °C
1330 ksi

@Strain 0.360 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® HR5330HFS NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
30% Glass Reinforced Polybutylene Terephthalate with Improved Processing Crastin HR5330HFS is a 30% glass fiber reinforced moderately toughened hydrolysis resistant polybutylene terephthalate for in..
Secant Modulus 9.20 GPa

@Strain 1.50 %,
Temperature -40.0 °C
1330 ksi

@Strain 1.50 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® LW9030 NC010 PBT+ASA  (Unverified Data**)
30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030 NC010 is a 30% glass fiber reinforced polybutylene terephthalate blend for injection molding. ..
Secant Modulus 9.18 GPa

@Strain 1.50 %,
Temperature -20.0 °C
1330 ksi

@Strain 1.50 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK645FR NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK645FR is a flame retardant 30% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.7..
Secant Modulus 9.19 GPa

@Strain 1.48 %,
Temperature 0.000 °C
1330 ksi

@Strain 1.48 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® FR530 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
30% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR530 NC010 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont ..
Secant Modulus 9.19 GPa

@Strain 1.30 %,
Temperature 23.0 °C
1330 ksi

@Strain 1.30 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 73G35HSL BK262 Nylon 6  (Unverified Data**)
35% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G35HSL BK262 is a 35% glass fiber reinforced heat stabilized black polyamide 6 resin for injection molding.Information provided by DuPont Per..