Polymer Property : Secant Modulus = 129 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 0.889 GPa

@Strain 3.80 %,
Temperature 80.0 °C
129 ksi

@Strain 3.80 %,
Temperature 176 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 511DP NC010 Acetal (POM)  (Unverified Data**)
Nucleated Medium Viscosity Acetal Homopolymer Delrin 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less s..
Secant Modulus 0.889 GPa

@Strain 3.80 %,
Temperature 80.0 °C
129 ksi

@Strain 3.80 %,
Temperature 176 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG511DP NC010 Acetal (POM)  (Unverified Data**)
Nucleated Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for mo..
Secant Modulus 0.887 GPa

@Strain 7.37 %,
Temperature 0.000 °C
129 ksi

@Strain 7.37 %,
Temperature 32.0 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS LC3060 NC010 Nylon 610  (Unverified Data**)
Unreinforced Renewably Sourced Medium Viscosity Polyamide 610 Developed for Extrusion Zytel RS LC3060 NC010 is a renewable sourced polyamide 610 containing a minimum of 60% renewable sourced ingredi..