Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.854 GPa @Strain 2.40 %, Temperature 100 °C |
124 ksi @Strain 2.40 %, Temperature 212 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100AL NC010 Acetal (POM)
(Unverified Data**) Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 100AL NC010 an unreinforced high viscosity lubricated acetal homopolymer resin containing an advanced system of lub.. |
|||
Secant Modulus | 0.857 GPa @Strain 11.0 %, Temperature -40.0 °C |
124 ksi @Strain 11.0 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500P BK602 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Improved ProcessingDelrin 500P BK602 is a general purpose medium viscosity black acetal homopolymer resin for injection molding. Delrin 500P has improved pro.. |
|||
Secant Modulus | 0.855 GPa @Strain 1.10 %, Temperature 80.0 °C |
124 ksi @Strain 1.10 %, Temperature 176 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500T NC010 Acetal (POM)
(Unverified Data**) Toughened Medium Viscosity Acetal Homopolymer Delrin 500T NC010 is a toughened medium viscosity acetal homopolymer resin with impact resistance similar to Delrin 100. It can be used in parts requiri.. |
|||
Secant Modulus | 0.854 GPa @Strain 2.40 %, Temperature 100 °C |
124 ksi @Strain 2.40 %, Temperature 212 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG100AL NC010 Acetal (POM)
(Unverified Data**) Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact Applications Delrin FG100AL is a high viscosity lubricated acetal homopolymer resin containing .. |
|||
Secant Modulus | 0.855 GPa @Strain 3.80 %, Temperature 80.0 °C |
124 ksi @Strain 3.80 %, Temperature 176 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 10B40 NC010 Nylon 66
(Unverified Data**) 40% Mineral Reinforced Polyamide 66Minlon 10B40 NC010 is a 40% mineral reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Secant Modulus | 0.853 GPa @Strain 10.82 %, Temperature -40.0 °C |
124 ksi @Strain 10.82 %, Temperature -40.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC3060 NC010 Nylon 610
(Unverified Data**) Unreinforced Renewably Sourced Medium Viscosity Polyamide 610 Developed for Extrusion Zytel RS LC3060 NC010 is a renewable sourced polyamide 610 containing a minimum of 60% renewable sourced ingredi.. |