Polymer Property : Secant Modulus = 123 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 0.850 GPa

@Strain 0.400 %,
Temperature 100 °C
123 ksi

@Strain 0.400 %,
Temperature 212 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500P BK602 Acetal (POM)  (Unverified Data**)
Medium Viscosity Acetal Homopolymer with Improved ProcessingDelrin 500P BK602 is a general purpose medium viscosity black acetal homopolymer resin for injection molding. Delrin 500P has improved pro..
Secant Modulus 0.846 GPa

@Strain 8.30 %,
Temperature -20.0 °C
123 ksi

@Strain 8.30 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500T NC010 Acetal (POM)  (Unverified Data**)
Toughened Medium Viscosity Acetal Homopolymer Delrin 500T NC010 is a toughened medium viscosity acetal homopolymer resin with impact resistance similar to Delrin 100. It can be used in parts requiri..
Secant Modulus 0.850 GPa

@Strain 0.800 %,
Temperature 100 °C
123 ksi

@Strain 0.800 %,
Temperature 212 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 520MP NC010 Acetal (POM)  (Unverified Data**)
20% Teflon® Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 520MP is a medium viscosity acetal homopolymer containing 20% Teflon PTFE Micropowder. It is designe..
Secant Modulus 0.850 GPa

@Strain 9.00 %,
Temperature 0.000 °C
123 ksi

@Strain 9.00 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 100 BK602 Acetal (POM)  (Unverified Data**)
High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and ..
Secant Modulus 0.845 GPa

@Strain 10.0 %,
Temperature 0.000 °C
123 ksi

@Strain 10.0 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500PE NC010 Acetal (POM)  (Unverified Data**)
Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE NC010 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi..
Secant Modulus 0.846 GPa

@Strain 6.80 %,
Temperature 100 °C
123 ksi

@Strain 6.80 %,
Temperature 212 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G13HS1L NC010 Nylon 66  (Unverified Data**)
13% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G13HS1L NC010 is a 13% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perfor..