Mechanical Properties Metric English Comments
Secant Modulus 12.1 GPa

@Strain 0.215 %,
Temperature -20.0 °C
1760 ksi

@Strain 0.215 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK645FR NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK645FR is a flame retardant 30% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.7..
Secant Modulus 12.1 GPa

@Strain 0.700 %,
Temperature -40.0 °C
1760 ksi

@Strain 0.700 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® FR530 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
30% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR530 NC010 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont ..
Secant Modulus 12.1 GPa

@Strain 1.52 %,
Temperature 23.0 °C
1750 ksi

@Strain 1.52 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 92G45DH2 BK083 Polyphthalamide (PPA)
35% Glass Reinforced PPA High Performance Polyamide with DuPont Zytel HTN92G45DH2 BK083 is a 45% glass reinforced high performance polyamide resin using DuPont SHIELD Technology with high flow and e..
Secant Modulus 12.1 GPa

@Strain 0.390 %,
Temperature -40.0 °C
1760 ksi

@Strain 0.390 %,
Temperature -40.0 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® EFE7374 BK416 Nylon 6  (Unverified Data**)
40% Glass Reinforced Toughened Polyamide 6 Zytel EFE7374 is a 40% fiber reinforced heat stabilized lubricated toughened polyamide 6 for injection molding. It has an improved impact resistance and ex..