Mechanical Properties Metric English Comments
Secant Modulus 10.1 GPa

@Strain 0.960 %,
Temperature -20.0 °C
1460 ksi

@Strain 0.960 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® LW9030FR NC010 PBT+ASA  (Unverified Data**)
30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030FR NC010 is a 30% glass fiber reinforced flame retardant polybutylene terephthal..
Secant Modulus 10.1 GPa

@Strain 0.770 %,
Temperature 0.000 °C
1470 ksi

@Strain 0.770 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® LW9030FR NC010 PBT+ASA  (Unverified Data**)
30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030FR NC010 is a 30% glass fiber reinforced flame retardant polybutylene terephthal..
Secant Modulus 10.1 GPa

@Strain 0.110 %,
Temperature -40.0 °C
1460 ksi

@Strain 0.110 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® 935SUV BK593 Polyethylene Terephthalate (PET)  (Unverified Data**)
35% Glass Reinforced UV Stabilized Polyethylene Terephthalate Rynite 935SUV BK593 is a 35% glass fiber /mineral reinforced UV stabilized modified polyethylene terephthalate resin with low warpage de..
Secant Modulus 10.1 GPa

@Strain 1.86 %,
Temperature 23.0 °C
1460 ksi

@Strain 1.86 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® RE5264 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
36% Glass Reinforced Polyethylene Terephthalate Rynite RE5264 NC010 is a 36% glass fiber reinforced color stabilized modified polyethylene terephthalate.Information provided by DuPont Performance Po..
Secant Modulus 10.1 GPa

@Strain 0.900 %,
Temperature -40.0 °C
1470 ksi

@Strain 0.900 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Sorona® 3030GV NC010 Polytrimethylene Terephthalate (PTT)
30% Glass Reinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3030GV NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on pol..
Secant Modulus 10.1 GPa

@Strain 1.10 %,
Temperature 23.0 °C
1470 ksi

@Strain 1.10 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® PLS 95G40DH1T BK261 Nylon 6  (Unverified Data**)
40% Glass Reinforced Heat Stabilized Polyamide Zytel PLS95G40DH1T is a 40% GR impact modified PA made with SHIELD technology its superior heatInformation provided by DuPont Performance Polymers
Secant Modulus 10.1 GPa

@Strain 0.900 %,
Temperature -40.0 °C
1470 ksi

@Strain 0.900 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Sorona® 3030G NC010 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)&
30% Glass Reinforced Polytrimethylene Terephthalate Sorona 3030G NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with goo..
Secant Modulus 10.1 GPa

@Strain 0.231655 %,
Temperature 0.000 °C
1460 ksi

@Strain 0.231655 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK615SF NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
30% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK615SF is a 30% glass fiber reinforced low viscosity polybutylene terephthalate for injecti..
Secant Modulus 10.1 GPa

@Strain 0.412778 %,
Temperature 23.0 °C
1460 ksi

@Strain 0.412778 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK615SF NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
30% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK615SF is a 30% glass fiber reinforced low viscosity polybutylene terephthalate for injecti..