Mechanical Properties Metric English Comments
Secant Modulus 1.95 GPa

@Strain 3.80 %,
Temperature -20.0 °C
282 ksi

@Strain 3.80 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® 6129 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection MoldingInformation provided by DuPont Performance Polymers
Secant Modulus 1.95 GPa

@Strain 3.80 %,
Temperature -20.0 °C
282 ksi

@Strain 3.80 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® 6130 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin 6130 NC010 is an unreinforced medium high viscosity polybutylene terephthalate resin for ..
Secant Modulus 1.95 GPa

@Strain 3.61 %,
Temperature -40.0 °C
283 ksi

@Strain 3.61 %,
Temperature -40.0 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS LC3090 NC010 Nylon 610  (Unverified Data**)
Unreinforced Renewably Sourced High Viscosity Polyamide 610 Developed for Extrusion Zytel RS LC3090 NC010 is a renewable sourced polyamide 610 containing a miniumu of 60% renewably sourced ingredien..
Secant Modulus 1.95 GPa

@Strain 1.60 %,
Temperature 100 °C
283 ksi

@Strain 1.60 %,
Temperature 212 °F
ISO 11403-1 -2
DuPont Performance Polymers Sorona® 3015G NC010 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)&
15% Glass Reinforced Polytrimethylene Terephthalate with Resin Made from Bio-PDO Sorona 3015G NC010 is a 15% glass reinforced PTT resin containing 31% renewably sourced ingredients by weight (37% ba..