Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 1.80 GPa @Strain 0.250 %, Temperature 80.0 °C |
261 ksi @Strain 0.250 %, Temperature 176 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK601 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 10% Glass Reinforced Polybutylene Terephthalate Crastin SK601 NC010 is a 10% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |
|||
Secant Modulus | 1.80 GPa @Strain 1.80 %, Temperature 23.0 °C |
261 ksi @Strain 1.80 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 520MP NC010 Acetal (POM)
(Unverified Data**) 20% Teflon® Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 520MP is a medium viscosity acetal homopolymer containing 20% Teflon PTFE Micropowder. It is designe.. |
|||
Secant Modulus | 1.80 GPa @Strain 2.70 %, Temperature 80.0 °C |
262 ksi @Strain 2.70 %, Temperature 176 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Sorona® 3015G NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& 15% Glass Reinforced Polytrimethylene Terephthalate with Resin Made from Bio-PDO Sorona 3015G NC010 is a 15% glass reinforced PTT resin containing 31% renewably sourced ingredients by weight (37% ba.. |