Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Secant Modulus = 1.67 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 1.67 GPa

@Strain 4.30 %,
Temperature 0.000 °C
242 ksi

@Strain 4.30 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500TL NC010 Acetal (POM)  (Unverified Data**)
Teflon® Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500TL is a medium viscosity acetal homopolymer resin containing 1.5% Teflon PTFE Micropowder. It is desi..
Secant Modulus 1.67 GPa

@Strain 4.40 %,
Temperature 0.000 °C
242 ksi

@Strain 4.40 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 511DP NC010 Acetal (POM)  (Unverified Data**)
Nucleated Medium Viscosity Acetal Homopolymer Delrin 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less s..
Secant Modulus 1.67 GPa

@Strain 4.50 %,
Temperature -20.0 °C
242 ksi

@Strain 4.50 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG500P NC010 Acetal (POM)  (Unverified Data**)
Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG500P is a medium viscosity acetal homopolymer with improved thermal stability. It has been developed for consider..
Secant Modulus 1.67 GPa

@Strain 4.30 %,
Temperature 0.000 °C
242 ksi

@Strain 4.30 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG500TL NC010 Acetal (POM)  (Unverified Data**)
Teflon® Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact ApplicationsDelrin FG500TL medium viscosity acetal homopolymer resin containing 1.5%..
Secant Modulus 1.67 GPa

@Strain 4.40 %,
Temperature 0.000 °C
242 ksi

@Strain 4.40 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG511DP NC010 Acetal (POM)  (Unverified Data**)
Nucleated Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for mo..
Secant Modulus 1.67 GPa

@Strain 4.84 %,
Temperature -20.0 °C
242 ksi

@Strain 4.84 %,
Temperature -4.00 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS LC3090 NC010 Nylon 610  (Unverified Data**)
Unreinforced Renewably Sourced High Viscosity Polyamide 610 Developed for Extrusion Zytel RS LC3090 NC010 is a renewable sourced polyamide 610 containing a miniumu of 60% renewably sourced ingredien..
Secant Modulus 1.67 GPa

@Strain 2.40 %,
Temperature 100 °C
243 ksi

@Strain 2.40 %,
Temperature 212 °F
ISO 11403-1 -2
DuPont Performance Polymers Sorona® 3015G NC010 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)&
15% Glass Reinforced Polytrimethylene Terephthalate with Resin Made from Bio-PDO Sorona 3015G NC010 is a 15% glass reinforced PTT resin containing 31% renewably sourced ingredients by weight (37% ba..
Copyright © lookpolymers.com All Rights Reserved