Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 1.55 GPa @Strain 6.14547 %, Temperature -40.0 °C |
225 ksi @Strain 6.14547 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® S600F10 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin S600F10 NC010 is an unreinforced lubricated medium high viscosity polybutylene terephthal.. |
|||
Secant Modulus | 1.55 GPa @Strain 1.40 %, Temperature 40.0 °C |
225 ksi @Strain 1.40 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500T NC010 Acetal (POM)
(Unverified Data**) Toughened Medium Viscosity Acetal Homopolymer Delrin 500T NC010 is a toughened medium viscosity acetal homopolymer resin with impact resistance similar to Delrin 100. It can be used in parts requiri.. |
|||
Secant Modulus | 1.55 GPa @Strain 3.87 %, Temperature 100 °C |
225 ksi @Strain 3.87 %, Temperature 212 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS 32CG20HSL BK409 Nylon 610
(Unverified Data**) 20% Carbon/Glass Reinforced Renewably Sourced Polyamide 610 Information provided by DuPont Performance Polymers |
|||
Secant Modulus | 1.55 GPa @Strain 2.40 %, Temperature 23.0 °C |
224 ksi @Strain 2.40 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® ST830FRUV NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Flame Retardant UV Stabilized Polybutylene Terephthalate Crastin ST830FRUV NC010 is an unreinforced Super Tough flame retardant polybutylene terephthalate resin for injection molding. I.. |
|||
Secant Modulus | 1.55 GPa @Strain 6.00 %, Temperature -40.0 °C |
225 ksi @Strain 6.00 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100 BK602 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and .. |