Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 1.50 GPa @Strain 1.38 %, Temperature 23.0 °C |
217 ksi @Strain 1.38 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® BM6450XD BK560 Polybutylene Terephthalate (PBT)
(Unverified Data**)& Unreinforced Polybutylene Terephthalate Developed for Blow MoldingCrastin BM6450XD BK560 is an unreinforced supertough polybutylene terephthalate resin with very high viscosity for extrusion and blo.. |
|||
Secant Modulus | 1.50 GPa @Strain 1.40 %, Temperature 100 °C |
217 ksi @Strain 1.40 %, Temperature 212 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 10B40 NC010 Nylon 66
(Unverified Data**) 40% Mineral Reinforced Polyamide 66Minlon 10B40 NC010 is a 40% mineral reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Secant Modulus | 1.50 GPa @Strain 4.30 %, Temperature 23.0 °C |
218 ksi @Strain 4.30 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500PE BK602 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE BK602 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi.. |