Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Secant Modulus = 0.417 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 0.417 GPa

@Strain 7.20 %,
Temperature 100 °C
60.4 ksi

@Strain 7.20 %,
Temperature 212 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 900P NC010 Acetal (POM)  (Unverified Data**)
Low Viscosity Acetal Homopolymer with Improved Processing Delrin 900P is a low viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical proper..
Secant Modulus 0.417 GPa

@Strain 7.20 %,
Temperature 100 °C
60.4 ksi

@Strain 7.20 %,
Temperature 212 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG900P NC010 Acetal (POM)  (Unverified Data**)
Low Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG900P is a low viscosity acetal homopolymer with improved thermal stability. It has been developed for consideration ..
Secant Modulus 0.417 GPa

@Strain 19.0 %,
Temperature 0.000 °C
60.5 ksi

@Strain 19.0 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 100 BK602 Acetal (POM)  (Unverified Data**)
High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and ..
Copyright © lookpolymers.com All Rights Reserved