Polymer Property : Compressive Modulus = 4.14 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 4.14 GPa
600 ksi
ASTM D695
Quadrant EPP Nylatron® GF30 Nylon Type 66, 30% Glass-Reinforced Black Color (ASTM Product Data Sheet)
Compressive Modulus 4.14 GPa
600 ksi
ASTM D695
Quadrant EPP Semitron® ESd 520HR (ASTM Product Data Sheet)
Compressive Modulus 4.14 GPa
600 ksi
ASTM D695
Quadrant EPP Semitron® MP-370 (ASTM Product Data Sheet)
Compressive Modulus 4.14 GPa
600 ksi
TM R050-38
Resinlab® EP1320LV Heat Cure Epoxy Conformal Coating
Resinlab™ EP1320 and EP1320LV are one part heat cure epoxy conformal coatings. They can also be used as a small mass potting compounds, structural adhesives, or insulating polymer systems where the..
Compressive Modulus 4.14 GPa
600 ksi
TM R050-38
Resinlab® EP1325 Thixotropic, Heat Curing Epoxy Adhesive
Resinlab™ EP1325 and EP1325LV are one part thixotropic, heat curing epoxy adhesives. They can also be used as a small mass potting compounds, staking or damming adhesives, or polymer systems where ..
Compressive Modulus 4.14 GPa
600 ksi
TM R050-38
Resinlab® EP1325LV Thixotropic, Heat Curing Epoxy Adhesive
Resinlab™ EP1325 and EP1325LV are one part thixotropic, heat curing epoxy adhesives. They can also be used as a small mass potting compounds, staking or damming adhesives, or polymer systems where ..
Compressive Modulus 4.14 GPa
600 ksi
ASTM D695
Quadrant EPP Duratron® PAI T5530 Compression Molded Glass Reinforced Polyamide-imide (ASTM Product Data Sheet)
Compressive Modulus 4.14 GPa
600 ksi
ASTM D695
Quadrant EPP Semitron® ESd 410C- CM Dissipative Polyetherimide(ASTM Product Data Sheet)
Compressive Modulus 4.14 GPa
600 ksi
ASTM D695
Quadrant EPP Semitron® ESd 490HR Static dissipative PEEK for use in test fixtures. Non-sloughing and low moisture absorption. (ASTM Product Data Sheet)
Compressive Modulus 4.14 - 7.93 GPa
600 - 1150 ksi
Average value: 5.63 GPa Grade Count:3
Overview of materials for Polyamide-Imide, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyamide-Imide, Glass Filled". Each property range of values reported is minimum and maximum values of ..
Compressive Modulus 4.14 GPa
600 ksi
ASTM D695
Ensinger Tecapeek® XP-98 Compression Molded PEEK Compound, 30% Carbon Fiber
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in..
Compressive Modulus 4.14 GPa
600 ksi
ASTM D695
Ensinger Tecapeek® XP-98 Medical Compression Molded PEEK Compound, 30% Carbon Fiber
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in..