Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.0710 GPa | 10.3 ksi | ASTM D1621 |
SABIC Innovative Plastics ULTEM Foam XP080 PEI ULTEM foam is a polyetherimide based thermoplastic foam with excellent flame, smoke and toxicity performance. The material combines a high strength to weight ratio with low moisture absorption. The .. |
|||
Compressive Modulus | 0.0710 GPa | 10.3 ksi | ASTM D1621 |
SABIC Innovative Plastics ULTEM Foam XP080 PEI (Asia Pacific) ULTEM foam is a polyetherimide based thermoplastic foam with excellent flame, smoke and toxicity performance. The material combines a high strength to weight ratio with low moisture absorption. The .. |