Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.0172 GPa | 2.49 ksi | ASTM D695 |
Quantum Composites QC-8560 60% Glass Fiber Vinyl Ester SMC QC-8560 is a vinyl ester based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength. It maintains excellent mechanical properties at temper.. |
|||
Compressive Modulus | 0.0172 - 33.8 GPa | 2.49 - 4900 ksi | Average value: 12.2 GPa Grade Count:7 |
Overview of materials for Vinyl Ester Sheet Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Vinyl Ester Sheet Molding Compound". Each property range of values reported is minimum and maximum value.. |