Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.0000614 GPa | 0.00890 ksi | Force to Compress; AAMA 810.1 |
Saint-Gobain Norton® V980 Paper Liner Pressure Sensitive Adhesive Foam Sealant Description: Closed cell PVC foam with a pressure-sensitive adhesive on both sides. Proven Performance: Norseal® V980/V990 foam sealant combines a closed cell polyvinyl chloride foam substrate wt.. |
|||
Compressive Modulus | 0.0000614 GPa | 0.00890 ksi | Force to Compress; AAMA 810.1 |
Saint-Gobain Norton® V990 Poly Liner Pressure Sensitive Adhesive Foam Sealant Description: Closed cell PVC foam with a pressure-sensitive adhesive on both sides. Proven Performance: Norseal® V980/V990 foam sealant combines a closed cell polyvinyl chloride foam substrate wt.. |