Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 89.63 MPa | 13000 psi | |
Abatron AboCast/AboCure 8109-10 2-part, clear, slow casting/impregnating dielectric compound. Low dielectric constant, good flexibility and thermocycling properties. Abocast 8502-4 is a red (and other colors), filled version.Pro.. |