Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 55.0 - 276 MPa | 7980 - 40000 psi | Average value: 179 MPa Grade Count:4 |
Overview of materials for Polyamide-Imide, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyamide-Imide, Glass Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Compressive Yield Strength | 55.0 MPa | 7980 psi | at 2% compression parallel to thickness |
Zircar Refractory Composites RS-1200 Refractory Sheet ZIRCAR Refractory Sheet Type RS-1200 is a high strength composite designed for use as thermo-mechanical and electrical insulation in applications with temperatures as high as 1300°C(2372°F). RS-12.. |
|||
Compressive Yield Strength | 55.0 MPa | 7980 psi | ASTM D695 |
Adell BI-10 Nylon 6, Impact Modified Data provided by Adell Plastics, Inc. |
|||
Compressive Yield Strength | 55.0 MPa | 7980 psi | ASTM D695 |
Adell BI-30 Nylon 6, Impact Modified Data provided by Adell Plastics, Inc. |